In the process of ordinary zipper bags, the following four problems are often encountered:
1. The two ends of the zipper the side seal of the bag intersect each other;
2. The part the two ends of the zipper intersect with the edge seal of the bag has local delamination;
3. The sealing part of zipper bag body is smooth;
4. The part of the zipper the bag body is partially delaminating;
The causes of the above four types of problems are as follows:
1. The design of local heat sealing head is unreasonable (too small);
2. Insufficient output power pressure of ultrasonic heat sealing device;
3. The hardness of silicone rubber pad is suitable;
4. The design of the local heat sealing rod on the zipper bag making machine is unreasonable, so it is suggested to use the ultrasonic heat sealing device;
5. The thermal shrinkage of zipper is larger than that of composite film;
6. The melting point of the zipper itself is greater than equal to that of the thermal seal film;
7. Lack of heat resistance of ink layer;
8. The cross section of the daughter mother buttons on the zipper is too large;